Title: | Does Delayed Restoration Improve Shear Bond Strength of Different Restorative Protocols to Calcium Silicate-Based Cements? | Authors: | Palma, Paulo J. Marques, Joana A. Falacho, Rui I. Vinagre, Alexandra Santos, João Miguel Ramos, João C. |
Keywords: | Biodentine; calcium silicate-based cements; mineral trioxide aggregate; regenerative endodontic procedures; shear bond strength; universal bonding agent | Issue Date: | 8-Nov-2018 | Publisher: | MDPI | metadata.degois.publication.title: | Materials | metadata.degois.publication.volume: | 11 | metadata.degois.publication.issue: | 11 | Abstract: | The purpose of the present study was to assess the proper time to perform a restoration (immediately or delayed) after placement of two calcium silicate-based cements (CSCs) and to test the performance of two different restorative protocols regarding shear bond strength (SBS). Seventy-five acrylic blocks were randomly divided into five groups (n = 15). Specimens were filled with either ProRoot MTA (Dentsply Tulsa Dental) or Biodentine (Septodont). The restoration was performed at an immediate (12 min) or delayed (seven days) timeframe, using a resin-based flowable composite (SDR) (bonded to the CSC using a universal bonding system) or glass ionomer cement (GIC) as restorative materials. SBS was measured using a universal testing machine. Fractured surfaces were evaluated, and the pattern was registered. Statistical analysis was performed using the Dunn⁻Sidak post hoc test (P < 0.05). Biodentine/immediate SDR showed the highest mean SBS value (4.44 MPa), with statistically significant differences when compared to mineral trioxide aggregate (MTA)/GIC (1.14 MPa) and MTA/immediate SDR (1.33 MPa). MTA/GIC and MTA/immediate SDR did not present significant differences regarding SBS. No statistical differences were verified concerning mean SBS between both CSCs within the 7 day groups. MTA/delayed SDR (3.86 MPa) presented statistical differences compared to MTA/immediate SDR, whereas no differences were observed regarding Biodentine performance (Biodentine/immediate SDR and Biodentine/delayed SDR (3.09 MPa)). Bonding procedures directly on top of MTA might be preferably performed at a delayed timeframe, whereas Biodentine might allow for immediate restoration. | URI: | https://hdl.handle.net/10316/113989 | ISSN: | 1996-1944 | DOI: | 10.3390/ma11112216 | Rights: | openAccess |
Appears in Collections: | FMUC Med. Dentária - Artigos em Revistas Internacionais |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
ArtigoMaterials-Does Delayed Restoration.pdf | 446.57 kB | Adobe PDF | View/Open |
Page view(s)
105
checked on Oct 30, 2024
Download(s)
16
checked on Oct 30, 2024
Google ScholarTM
Check
Altmetric
Altmetric
This item is licensed under a Creative Commons License